PG-200/300 Bitumen

No.Test ItemsMethodsSpec
1Penetration @ 25◦CASTM D 5200/300
2Flash Point ASTM D 92Min 175
3Solubility in TCEASTM D 2042Min 99
4Density at 25◦c, kg/m3ASTM D 701.01-1.06
5Ductility@ 25◦CASTM D 113Min 100
6Spot Test A.A.S.H.T.O T102 Negative
7Softening PointASTM D 36Min 32
AFTER THIN FILM OVEN TEST , ASTM D1754
8Change mass wt%ASTM D1754max 1/5
9Retain penetration at 25◦c%ASTM D1754:D5min 37%
10Ductility at 25◦c, cmASTM D1754:D113min100